发明名称 |
Process for producing an intermetallic join |
摘要 |
PCT No. PCT/DE96/01808 Sec. 371 Date Mar. 31, 1998 Sec. 102(e) Date Mar. 31, 1998 PCT Filed Sep. 20, 1996 PCT Pub. No. WO97/13597 PCT Pub. Date Apr. 17, 1997The aim is to improve the strength of an intermetallic bond between engine component made from an aluminium alloy and a reinforcing element made from austenitic cast iron. For that purpose, the reinforcing element is annealed in a decarbonising atmosphere before the known prior art alfin process is carried out, in order to obtain an alfin layer largely free of graphite scales.
|
申请公布号 |
US6112802(A) |
申请公布日期 |
2000.09.05 |
申请号 |
US19980051050 |
申请日期 |
1998.03.31 |
申请人 |
MAHLE GMBH |
发明人 |
HUDELMAIER, BIRGIT;MUELLER-SCHWELLING, DIETER;SCHLOSSER, DETLEF |
分类号 |
F02F5/00;B22D19/00;B22D19/04;B22D19/16;B22D21/04;F02F7/00;F16J1/01;(IPC1-7):B22D19/00;F02F3/00 |
主分类号 |
F02F5/00 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|