<p>PROBLEM TO BE SOLVED: To prepare a processing agent for textile products, effective in restoration of the shape and feeling of deteriorated clothing by formulating a water soluble polymer having a specific range of a weight average molecular weight and an amino-modified silicone compound. SOLUTION: This processing agent for textile products is prepared by the formulation of (A) 0.1-30 wt.% (preferably 1-15 wt.%) water soluble polymer selected from the group consisting of water soluble modified starch (or its derivative), a water soluble cellulose derivative and a N-vinyl-2-pyrrolidone-based (co)polymer, each having 5,000-500,000 weight average molecular weight, (B) 0.05-10 wt.% (preferably 0.5-8 wt.%) amino-modified silicone compound having 1,000-1,000,000 weight average molecular weight (preferably 2,000-100,000 weight average molecular weight) and (C) 0.1-5 wt.% (preferably 0.3-3 wt.%) nonionic surfactant.</p> |