摘要 |
PROBLEM TO BE SOLVED: To provide a recording sheet having no subdued print and fast coating film. SOLUTION: In the recording sheet, an ink receptive layer is formed on at least one surface of a base material. The layer contains a component (1) exhibiting water solubility in a molecule and a component (2) containing a functional group for forming a crosslinking point in a molecule, and contains a resin (a) exhibiting water solubility before forming the point, and a polymer (b) of predetermined polymer electrolyte. As the electrolyte (b), for example, an acrylic polymer containing a quaternary ammonium salt having a carboxylic acid group is used. A blending ratio of the resin (a) to the polymer (b) in the layer is preferably in a range of 20:80 to 40:60, and more preferably 25:70 to 35:65. |