发明名称 Pulverized coal carriability improver
摘要 PCT No. PCT/JP97/00668 Sec. 371 Date Sep. 25, 1998 Sec. 102(e) Date Sep. 25, 1998 PCT Filed Mar. 5, 1997 PCT Pub. No. WO97/36009 PCT Pub. Date Oct. 2, 1997The use of pulverized coal as the fuel to be injected into metallurgical or combustion furnace becomes possible enabled by improving the transportability thereof. Further, a pulverized coal is provided, which is inhibiting from bridging or channeling in a hopper, or piping choking. A water-soluble inorganic salt having a polar group is made to adhere to pulverized coal which is prepared from raw coal having an average HGI of 30 or above and which is in a dry state at the injection port of a metallurgical or combustion furnace, The inorganic salt is selected from among BaCl2, CaCl2, Ca(NO2)2, Ca(NO3)2, Ca(ClO)2, K2CO3, KCl, MgCl2, MgSO4, NH4BF4, NH4Cl, (NH4)2SO4, Na2CO3, NaCl, NaClO3, NaNO2, NaNO3, NaOH, Na2S2O3, Na2S2O5, HNO3, H2SO4, H2CO3, and HCl.
申请公布号 US6083289(A) 申请公布日期 2000.07.04
申请号 US19980155296 申请日期 1998.09.25
申请人 KAO CORPORATION 发明人 ONO, REIJI;NAKAYA, TAKASHI;KIMURA, YOSHIO;KAMIJO, TSUNAO;MIYAMOTO, KENICHI;MATOBA, TAKASHI;OHASHI, HIDEMI;ICHIMOTO, TAKEHIKO
分类号 F23C99/00;C10L5/00;C21B5/00;F23K1/00;F23K3/00;F23K3/02;(IPC1-7):C10L9/10 主分类号 F23C99/00
代理机构 代理人
主权项
地址