摘要 |
FIELD: polymer production. SUBSTANCE: coating area (where polymerization has to be initiated) is irradiated by way of N-fold scanning with initiation emission beam at beam travel velocity m-fold superior to polymerization initiation velocity with single scanning, provided that m > N. Method is suitable for stereolithography, drying of paint, adhesive, protective, and decorative coatings when manufacturing optical disks, light guides, and printing plates. EFFECT: enhanced polymerization initiation efficiency with use of radiation sources owing to reduced emission power and time consumption. 2 tbl, 2 dwg
|