PROBLEM TO BE SOLVED: To provide an economical skin for foam free from risk of environmen tal pollution, hardly generating surface discoloration over a long period of time, not generating wrinkles or demolding inferiority at the time of powder slush molding and not requiring coating agent treatment for preventing damage. SOLUTION: In a skin 10 consisting of two layers comprising a powder slush molded product covering the surface of a foam, a first layer 11 becoming an outer layer comprises a thermoplastic polyurethane resin containing an isocyanate component being an aliphatic or acyclic isocyanate and a second layer 13 becoming a foam side comprises a thermoplastic polyurethane resin containing an isocyanate component being an aromatic isocyanate. |