摘要 |
PROBLEM TO BE SOLVED: To provide a method for compounding superfine coke with sintered raw material which makes it possible to utilize the superfine coke recovered when collecting dust for carbonaceous material for production of sintered ore. SOLUTION: The iron ore powders for production of the sintered ore is prepared by piling many brands of the iron ore powders in multiple layers on a yard 1 of a rectangular shape in its base surface, feeding the iron ore powders by a reclaimer to a direction orthogonal with the axis of the rectangular shape and uniformly mixing these powders. At this time, the superfine coke 1 is first moistened and thereafter the layers of a uniform thickness are formed on the ground surface of the yard and the iron ore powders are successively stacked thereon so as to cover the superfine coke layers.
|