发明名称 VERTICAL DOWNWARD BUILD-UP WELDING METHOD
摘要 PROBLEM TO BE SOLVED: To make penetration shallow even in the case of a high welding current and to increase the speed of build-up welding by vertically and downward advancing, while rotating a welding wire in a high speed in a shield gas atmosphere and conducting build-up welding on a metal panel surface vertically held. SOLUTION: The material of a welding wire is preferably a nickel base alloy, a shield gas is preferably argon or an argon based mixture gas. A rotation diameter of a wire tip is set to 2-5 mm, a rotation speed to 10-60 Hz. A welding power source is that an average electric current is a pulse current of 200-240 A or a DC of 220-280 A. A welding voltage is preferably 27-32 V. A welding speed is preferably 1-1.3 m/min. A dilution rate of a nickel base alloy by welding is preferably <=20%. A welding speed as well as a welding current are made larger, welding efficiency is improved, the penetration is made shallow, the dilution rate is lowered, the corrosion resistance of a welded face is improved.
申请公布号 JP2000084665(A) 申请公布日期 2000.03.28
申请号 JP19980254707 申请日期 1998.09.09
申请人 NKK CORP 发明人 SANO TAKANOBU;MO BUNKETSU
分类号 B23K9/04;B23K9/00;B23K9/09;(IPC1-7):B23K9/04 主分类号 B23K9/04
代理机构 代理人
主权项
地址