发明名称 PRODUCTION OF MOLDED BODY
摘要 PROBLEM TO BE SOLVED: To improve strength by mixing polyethylene, reactive polyethylene and vegetable substance, then melting and molding. SOLUTION: Normal polyethylene and reactive polyethylene are mixed, and the mixture polyethylene is heated to a temp. higher than the melting point and kept at that temp. (e.g. at 150 deg.C for 7.5 min). Then the mixture as melted is kneaded. Chlorella dried or processed in a pellet or powder form are mixed to the mixture polyethylene melt, kneaded at high temp. (e.g. at 160 deg.C for 7.5 min) to obtain a homogeneous mixture, which is then cooled. The mixture is formed into pellets. By forming the product as pellets, it can be easily handled and the homogeneity of the mixture is improved. Then the mixture as pellets is supplied to fill a molding die, melted and molded. The molding temp. and molding pressure are controlled to 150 to 190 deg.C and 1 to 7 MPa, respectively. Further, if necessary, the molded body is again put in the die, repressurized and cooled so as to stabilize the quality of the molded body.
申请公布号 JP2000070914(A) 申请公布日期 2000.03.07
申请号 JP19980246339 申请日期 1998.08.31
申请人 AGENCY OF IND SCIENCE & TECHNOL;RESEARCH INSTITUTE OF INNOVATIVE TECHNOLOGY FOR THE EARTH;ISHIKAWAJIMA HARIMA HEAVY IND CO LTD 发明人 CHO HATSUJO;HIROTSU TAKAHIRO;YAMASHITA MASATADA;OTSUKI TOSHI;KABETANI HIROSHI
分类号 B09B5/00;B29C43/02;B29K23/00;C08K5/09;C08K5/14;C08L1/02;C08L23/04;C08L23/26;(IPC1-7):B09B5/00 主分类号 B09B5/00
代理机构 代理人
主权项
地址