发明名称 Method of reducing metal oxide in a rotary hearth furnace heated by an oxidizing flame
摘要 <p>Method of reducing metal oxide using a furnace having an annular platform and at least one fuel burner involves: (i) placing a mixt. contg. the oxide and a reductant on the platform as a first layer; (ii) rotating the platform past a burner to heat the first layer with an oxidizing flame; (iii) covering the first layer with a second layer of reductant; and (iv) heating both layers to at least partially reduce the mixt.. The second layer prevents reoxidation of the partially reduced first layer. Also claimed are: (a) a method as identified above but where in step (ii) the first layer is heated to 1000[deg]C. and in step (iv) both layers are heated for 30 mins., where the partially reduced mixt. contains at least 1% metal; and (b) a method of reducing oxygen-bound iron and chromium.</p>
申请公布号 EP0747491(B1) 申请公布日期 2000.02.16
申请号 EP19960108322 申请日期 1996.05.24
申请人 ARMCO INC. 发明人 KUNDRAT, DAVID M.
分类号 C21B13/08;C21B13/10;C21C5/00;C22B5/10;C22C33/00;C22C35/00;(IPC1-7):C21C5/00 主分类号 C21B13/08
代理机构 代理人
主权项
地址