发明名称 CORNER CRACKING PREVENTING METHOD FOR STEEL PIECE
摘要 PROBLEM TO BE SOLVED: To prevent a corner cracking of steel pieces such as a billet without lowering a casting velocity by cooling a portion which is within a given %, of the side length and apart from a corner by a given % or more of the side length per side of a steel piece cross section as a range to be directly cooled. SOLUTION: According to a continuous casting machine, after a molten steel in a ladle is once poured into a tundish, the molten steel is flowed into a mold via a nozzle per strand. Simultaneously with the solidification of a surface, a steel piece 16 is pulled out by a roller while being gradually cooled by a secondary cooling water 15 for carrying out continuous casting. At the time of secondary cooling of the steel piece 16 being cast by the continuous casting device, corner cracking of the steel piece 16 is prevented by cooling the portion which is within 80% of one side length W1 and apart from a corner portion 16a by 10% or more of the side length per side of the steel piece 16 cross section.
申请公布号 JP2000005855(A) 申请公布日期 2000.01.11
申请号 JP19980177108 申请日期 1998.06.24
申请人 TOKAI KOGYO KK;NITTETSU OSAKA ENGINEERING KK 发明人 KANEMOTO MICHITAKA;TAMASHIMA SEIJI;HORIUCHI YASUSHI;YAMAMURO TAKASHI
分类号 B21B1/00;B21B45/08;B22D11/04;B22D11/22;(IPC1-7):B22D11/22 主分类号 B21B1/00
代理机构 代理人
主权项
地址