发明名称 |
Flux for brazing aluminum members |
摘要 |
A flux for brazing aluminum members comprising potassium tetrafluoroaluminate, potassium pentafluoroaluminate and oxyfluoroaluminum, accomplishing the brazing of aluminum members at temperatures 5 DEG C. to 20 DEG C. lower than the temperature of conventional brazing that uses fluoride fluxes. Thus, heating energy required for the brazing can thus be saved, and conventional brazing equipment can be used as it is, in principle, without any changes; and since no expensive elements are used in the fluxes, the cost of brazing aluminum members can be reduced.
|
申请公布号 |
US6010578(A) |
申请公布日期 |
2000.01.04 |
申请号 |
US19970977228 |
申请日期 |
1997.11.24 |
申请人 |
MORITA CHEMICAL INDUSTRY CO., LTD. |
发明人 |
ONO, MAKOTO;HATTORI, MASAHIRO;ITAYA, EIJI;YANAGAWA, YUTAKA |
分类号 |
B23K1/19;B23K35/36;B23K35/363;(IPC1-7):B23K35/363 |
主分类号 |
B23K1/19 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|