摘要 |
Copolymers of polyaspartic acid which are suitable for the inhibition of scale deposition were obtained by reacting maleic acid, an additional polycarboxylic acid and ammonia in a stoichiometric excess, at 120 DEG -350 DEG C., preferably 180 DEG -300 DEG C., to provide copolymers of polysuccinimide. In a second embodiment, a polyamine was added to the reaction mix. These intermediate polysuccinimide copolymers could then be converted to the salts of copolymers of polyaspartic acid by hydrolysis with a hydroxide. Such copolymers are useful in preventing deposition of scale from water and find applications in treating water. Other applications include scale prevention additives for detergents. In addition, such copolymers inhibit dental tartar and plaque formation.
|