发明名称 |
Lean, high conductivity, relaxation-resistant beryllium-nickel-copper alloys |
摘要 |
A higher order beryllium-nickel-copper alloy a process for making the same, and an article of manufacture comprising the alloy, the alloy being represented by the formula (0.15-0.5% Be)+(0.40-1.25% Ni)+(0-0.25% Sn)+[(0.06-1% Zr) and/or (0.06-1% Ti)], the balance copper, where the sum of % Zr and % Ti is generally within a range of 0.06% and 1%, the alloy being characterized by improved electrical conductivity, bend formability and stress relaxation resistance without sacrificing strength. |
申请公布号 |
US5993574(A) |
申请公布日期 |
1999.11.30 |
申请号 |
US19970965878 |
申请日期 |
1997.11.07 |
申请人 |
BRUSH WELLMAN, INC. |
发明人 |
HARKNESS, JOHN C.;WOLF, SHELLEY J. |