摘要 |
In a method for kneading a silane coupling agent-blended rubber composition prepared by blending a natural rubber and/or a diene group synthetic rubber with silica and a silane coupling agent, a coupling reaction of the silica with the silane coupling agent is carried out in a temperature range of 130 to 140 DEG C.
|