摘要 |
PROBLEM TO BE SOLVED: To prevent an invasion of moisture or vapor, and restrict an increase in a defect on external appearance of a solar cell module and enhance safety and reliability by a method wherein, when the solar cell module is scratched, the scratch is covered with a repair member. SOLUTION: A scratch 103 is covered with a repair member 104. Sunshines are incident on a sealing material 101, and reach a photoelectromotive element 102 to cause an electromotive force. The scratches 103 are dents, cuts, abrasions or the like caused in a sealing material of the solar cell module. There are some cases where fine splits of the sealing material or releasing of the sealing material is accompanied. The repair member 104 has weather-resistance, transparency and mechanical strength similar to those of the sealing material, and has an adhesiveness excellent in the sealing material of the solar cell module. Thus, it is possible to prevent an invasion of moisture or steam, and restrict an increase in a defect on external appearance of the solar cell module and enhance safety and reliability. Further, it has no adverse effect on performance of the solar cell module, and reliability equal to a product which has no repair members can be ensured. |