摘要 FIELD: building materials industry, more particularly applying fireproof coating onto metallic surfaces. SUBSTANCE: raw mix comprises, wt %: liquid glass, 65-77; sodium hydroxide, 2.1-3.1; aluminium sulfate, 1.73-2.1; zeolite 6.1-8.2; and the water balance. Characteristics of composition and coating; adhesion power is 1 mark; moisture resistance is 3.6- 3.7%; fire resistance is 3 hours; vibration resistance is 12-12,4 months; service time is more than 5 years; consumption per 1 sq.m is 7.2-7.8 kg; fitness period of raw mix is 1 year; corrosion resistance is 12 months. EFFECT: higher moisture and fire resistance. 3 tbl
申请公布号 RU2140401(C1) 申请公布日期 1999.10.27
申请号 RU19980122936 申请日期 1998.12.24
申请人 ARTEMENKO NIKOLAJ FEDOROVICH;BELEN'KIJ VLADISLAV MIKHAJLOVICH;IVANOV ALEKSANDR KONSTANTINOVICH;ISTJUKOV GENNADIJ NIKOLAEVICH;KALASHNIKOV NIKOLAJ GRIGOR'EVICH;MASLOV VLADIMIR ALEKSEEVICH;MEL'NIKOV VLADIMIR FEDOROVICH;KHEVSURIANI PLATON MIKHAJLOVICH 发明人 ARTEMENKO N.F.;BELEN'KIJ V.M.;IVANOV A.K.;ISTJUKOV G.N.;KALASHNIKOV N.G.;MASLOV V.A.;MEL'NIKOV V.F.;KHEVSURIANI P.M.
分类号 C04B28/26;C04B111/20;C09D1/02;(IPC1-7):C04B28/26 主分类号 C04B28/26
代理机构 代理人
主权项
地址
您可能感兴趣的专利