发明名称 ALUMINUM ALLOY WITH RESISTANCE TO HEAT AND WEAR, AND ITS PRODUCTION
摘要 PROBLEM TO BE SOLVED: To produce an aluminum alloy excellent in heat resistance and wear resistance, and its production. SOLUTION: This aluminum alloy has a composition consisting of, by mass, 10-30% Si, 1-5% Ti, 3-10%, in total, of at least either of Fe and Ni, 0.05-1.0% Mg, and the balance essentially Al. Further, the average crystalline grain size of Si is <=2μm, and the average grain size of intermetallic compound phases other than Si is <=1μm.
申请公布号 JPH11293374(A) 申请公布日期 1999.10.26
申请号 JP19980116135 申请日期 1998.04.10
申请人 SUMITOMO ELECTRIC IND LTD 发明人 KAJI TOSHIHIKO;HATTORI HISAO;HASHIKURA MANABU;TAKEDA YOSHINOBU
分类号 F02F3/00;B22F3/02;B22F3/17;C22C1/04;C22C1/10;C22C21/02;C22C32/00;(IPC1-7):C22C21/02 主分类号 F02F3/00
代理机构 代理人
主权项
地址