发明名称 STYRENIC RESIN COMPOSITION FOR EXTRUSION MOLDING AND MOLDED BODY
摘要 PROBLEM TO BE SOLVED: To obtain a composition with excellent balance between melt tension and fluidity by admixing at least one wax and a fatty acid metal salt with a resin composition comprising a styrenic resin and a filler in a specific wt. ratio thereby adjusting the melt tension to a specific value. SOLUTION: There are admixed 0.1-10 pts.wt. of at least one wax and 0.1-5 pts.wt. of at least one selected from salts of a fatty acid with Na, Mg, Ca and Al with 100 pts.wt. of a resin composition comprising 40-95 wt.% of a styrenic resin having an MFR of 0.1-80 such as a polystyrene, an acrylonitrile/ styrene resin or the like and 5-60 wt.% of at least one filler selected from metal oxides, metal carbonates, metal sulfates and the like to give a resin composition having a melt tension of 5-150 g. As the wax is employed a polyethylene wax having a viscosity at 140 deg.C of 100-30,000 cps, a polypropylene wax having a viscosity at 160 deg.C of 50-5,000 cps, an oxidized polyethylene wax having a viscosity at 140 deg.C of 100-30,000 cps or the like.
申请公布号 JPH11293071(A) 申请公布日期 1999.10.26
申请号 JP19980096035 申请日期 1998.04.08
申请人 ASAHI CHEM IND CO LTD 发明人 TAKAMI YASUHIKO
分类号 C08J9/04;B29C44/00;B29C47/00;B29C67/20;B29K25/00;B29K55/02;B29K96/02;B29K105/04;B29K105/16;B29L31/58;C08K3/04;C08K3/22;C08K3/24;C08K3/26;C08K3/34;C08K5/098;C08L25/00;C08L51/04;C08L55/02;(IPC1-7):C08L25/00 主分类号 C08J9/04
代理机构 代理人
主权项
地址