发明名称 Low thermal expansion coefficient lithium-, aluminum-, silicon- and oxygen-containing ceramic material
摘要 A lithium-, aluminum-, silicon- and oxygen-containing ceramic material is produced by mixing a pre-sintered mixture of a clay and a lithium-containing material with further clay and sintering. A ceramic material, containing lithium, aluminum, silicon and oxygen, is produced by: (a) preparing a first starting mixture of an aluminum- and silicon-containing clay and a lithium-containing material; (b) pre-sintering and optionally grinding the mixture; (c) preparing a second mixture of the pre-sintered material and an aluminum- and silicon-containing clay; and (d) sintering to form the ceramic material. Independent claims are also included for the following: (i) a ceramic material which comprises Li2O, Al2O3, SiOx (x = 1 to 2) and K2O and/or Na2O and which has a thermal expansion coefficient (100-1000 deg C) of -0.030 to +0.030; and (ii) a semifinished material which is suitable for ceramic material production and which comprises the product of step (b) in the above process.
申请公布号 DE19910548(A1) 申请公布日期 1999.10.14
申请号 DE19991010548 申请日期 1999.03.10
申请人 HUND, ADRIAAN CORNELIS CHRISTIAAN 发明人 HUND, ADRIAAN CORNELIS CHRISTIAAN
分类号 C04B35/19;(IPC1-7):C04B35/01;C04B35/18;C04B35/64 主分类号 C04B35/19
代理机构 代理人
主权项
地址
您可能感兴趣的专利