摘要 PURPOSE:To obtain elastic woven fabric having high extensibility and high recovery of extensibility by weaving yarn using latently crimping conjugate type polyester yarn capable of developing specific crimping performance as warp and/or weft and weaving. CONSTITUTION:Multifilament or yarn such as spun yarn comprising latently crimping conjugate polyester yarn developing crimp such as spiral crimp caused by difference in boil water shrinkage between a first component having crimping performance having >=70% modulus of elasticity and >=50% crimp ratio 30 minutes after boiling water treatment and a second component is formed. The yarn is used as warp and/or weft and woven to give woven fabric, which is subjected to 5-40% alkali weight loss treatment, dyed and finished under a condition of providing wet heat at 100 deg.C for >=30 minutes and crimp having the crimping performance is developed in the latently crimping conjugate type polyester yarn constituting the woven fabric to supply the woven fabric with elasticity.
申请公布号 JP2953539(B2) 申请公布日期 1999.09.27
申请号 JP19910102098 申请日期 1991.04.05
申请人 YUNICHIKA KK 发明人 KAMAMOTO KENTARO;HIBINO TOSHIHIDE;OKAMOTO YOSHIHISA;ABE KAZUNORI
分类号 D01F8/14;D03D15/04;D03D15/08;D06M11/00;D06M11/38;D06M101/00;D06M101/16;D06M101/30;D06M101/32;D06P5/00;(IPC1-7):D06M11/38 主分类号 D01F8/14
代理机构 代理人
主权项
地址