摘要 PROBLEM TO BE SOLVED: To provide a suspended grout compsn. which is injected for the purpose of soil improvement, such as prevention of liquefaction, slip failure, and uneven settlement, exhibits a permanent ground solidification function, is excellent in on-site primary dispersion stability, and has both high-speed penetrating properties and quick solidification properties. SOLUTION: This grout contains (A) quenched blast furnace slag having a 95 wt.% particle size (on a particle size integration curve) of at most 15μm and a specific surface area in a range of 0. 85-3 m<2> /g, (B) slaked lime having a 95 wt.% particle size (on a particle size integration curve) of 30μm or lower and a specific surface area in a range of 1-50 m<2> /g, (C) an inorg. alkali metal carbonate, and (D) an org. polymeric dispersion aid which has an inertia square radius of at least 150Åin a dilute (0.01-1 wt.%) aq. soln., the ratio of water/(slaked lime + quenched blast furnace slag) being 1-6, the ratio of the dispersion aid/(slaked lime + quenched blast furnace slag) being 0.005-0.05, and the ratio of the alkali metal carbonate/quenched blast furnace slag being 0.02-0.5.
申请公布号 JPH11228960(A) 申请公布日期 1999.08.24
申请号 JP19980028861 申请日期 1998.02.10
申请人 MITSUI CHEM INC 发明人 KITAMURA TADASHI;NAGATA MASAHIKO
分类号 E02D3/12;C09K17/02;C09K17/06;C09K103/00;(IPC1-7):C09K17/02 主分类号 E02D3/12
代理机构 代理人
主权项
地址