发明名称 METHOD OF HARDENING OF STEEL PARTS
摘要 FIELD: metallurgy; applicable in hardening of machine parts by method of cold plastic deformation for operation under conditions of friction and cyclic loads. SUBSTANCE: method includes prior to finishing thermo-chemical treatment - ionic nitriding, performance of prerecrystallization stabilizing annealing at temperatures exceeding temperature of maximum deformation ageing for the given steel grade by 80-120 C. This is made to preserve deformation hardening produced in material of part during cold plastic deformation. Such intermediate annealing ensures higher resistance of deformed steel to recrystallization in repeated heating. The method allows preservation of considerable part of metal deformation hardening in nitriding after annealing to increase strength properties of part core by 25-50% without appreciable reduction of ductility, and improved cyclic strength of finished article. EFFECT: higher efficiency. 1 dwg, 2 tbl
申请公布号 RU2134726(C1) 申请公布日期 1999.08.20
申请号 RU19970100860 申请日期 1997.01.28
申请人 AFANAS'EVA OL'GA VALENTINOVNA;GRABOV ANATOLIJ ALEKSANDROVICH;D'JACHENKO SVETLANA STEPANOVNA;ZOLOT'KO VLADIMIR ALEKSANDROVICH;KAFTANOV SERGEJ VLADIMIROVICH 发明人 AFANAS'EVA OL'GA VALENTINOVNA;GRABOV ANATOLIJ ALEKSANDROVICH;D'JACHENKO SVETLANA STEPANOVNA;ZOLOT'KO VLADIMIR ALEKSANDROVICH;KAFTANOV SERGEJ VLADIMIROVICH
分类号 C21D8/00;C21D1/78;C21D10/00;(IPC1-7):C21D8/00 主分类号 C21D8/00
代理机构 代理人
主权项
地址