发明名称 Manufacturing process of polyether-ester amide elastomer and elastic fiber
摘要 A manufacturing process of continuously producing a polyether-ester amide elastomer, which is adapted for mass production and reducing manufacturing cost, includes the steps of melting a poly (tetra methylene ether) glycol reactant, a epsilon -caprolactam reactant and an adipic acid reactant, pre-polymerizing the melted reactants by esterification and ring-opening reaction to form a pre-polymer and highly polymerizing the pre-polymer to form the polyether-ester amide elastomer. The polyether-ester amide elastomer is specifically used as a raw ingredient for producing a polyether-ester amide elastic fiber by drying the polyether-ester amide elastomer in a drying device, extruding the dried polyether-ester amide elastomer by an extruder, and molten spinning the extruded polyether-ester amide elastomer to form the polyether-ester amide elastic fiber.
申请公布号 US5917000(A) 申请公布日期 1999.06.29
申请号 US19980070108 申请日期 1998.04.29
申请人 TSAI, J. H.;CHIOU, J. S.;TWU, Y. K 发明人 TSAI, J. H.;CHIOU, J. S.;TWU, Y. K
分类号 C08G69/44;D01F6/86;(IPC1-7):C08G63/44 主分类号 C08G69/44
代理机构 代理人
主权项
地址