摘要 A method for preparing a lithiated transition metal oxide electrochemical charge storage material for use in an electrochemical cell. The cell (10) includes a cathode (20), an anode (30) and an electrolyte (40) disposed therebetween. The method involves the preparation of the lithiated, transition metal oxide material in an inert environment. The materials are characterized by improved electrochemical performance, and an identifiable x-ray diffraction matter.