<p>The hardness and appearance of an in-mold coating for a molded article of cured unsaturated polyester are improved by the addition of melamine and/or benzoguanamine to an unsaturated polyester powder coating composition and subjecting the modified powder coating to a molding temperature of from 126.5-171 DEG C and a pressure of from 4.48 to 13.8 MPa for 1 to 12 minutes. From 5 to 40 parts of the melamine and/or benzoguanamine per hundred parts by weight of the coating resin is preferably used.</p>
申请公布号
DE69324844(D1)
申请公布日期
1999.06.17
申请号
DE1993624844
申请日期
1993.02.19
申请人
MORTON INTERNATIONAL, INC., CHICAGO, ILL., US
发明人
RICHART, DOUGLAS S., READING, PENNSYLVANIA 19606, US