摘要 |
<p>A process for improving smoke quality and mechanical properties of a cast reconstituted tobacco sheet is accomplished by adding tobacco materials to an aqueous solution containing ammonium salts and ammonium hydroxide. The resulting first tobacco slurry is then pressurized under steam pressure to at least 60 psi for a period of from about 1 to 5 minutes then depressurized rapidly to ambient. The depressurized tobacco is then formed into a second tobacco slurry. The resulting tobacco residue is then cast into a reconstituted tobacco sheet for further processing into smoking articles.</p> |