发明名称 NON-SINTERED NICKEL ELECTRODE FOR SEALED ALKALINE STORAGE BATTERY
摘要 PROBLEM TO BE SOLVED: To increase the discharge capacity in a high-rate discharge of a battery by adding cobalt oxyhydroxide to a nickel hydroxide at a specified ratio, and setting the average valence of Ni in the nickel hydroxide to a specified value. SOLUTION: A nickel electrode contains 1-10 wt.% in terms of cobalt atom of cobalt oxyhydroxide to a nickel hydroxide of active material. As a positive electrode active material, a nickel hydroxide having an average valence of Ni of 2.1-2.3 is used. The nickel hydroxide having an average valence of Ni within this range can be manufactured easily, for example, by dipping nickel hydroxide in an aqueous solution obtained by adding an alkali to a strong oxidant aqueous solution, such as hydrogen peroxide for a prescribed time. When one or more elements selected from among Zn, Mg, Ca, Mn, Al, Cd, Y, Co, Bi and lanthanoids is solid dissolved to this nickel hydroxide, swelling of the possible electrode active material can be suppressed.
申请公布号 JPH11144723(A) 申请公布日期 1999.05.28
申请号 JP19970320480 申请日期 1997.11.05
申请人 SANYO ELECTRIC CO LTD 发明人 TOKUDA MITSUNORI;YANO MUTSUMI;FUJITANI SHIN;NISHIO KOJI
分类号 H01M4/52;H01M4/32;H01M4/62 主分类号 H01M4/52
代理机构 代理人
主权项
地址