发明名称 Sacrificial body for aluminum oxide-titanium aluminide composite body production by molten aluminum filling
摘要 A sacrificial body, for subsequent production of an alumina / titanium aluminide composite body, is formed by subjecting a starting mixture of titanium (especially as titanium oxide), carbon (precursor), filler and binder to pressing and heat treatment at below the subsequent aluminum filling temperature so that the filler and/or binder are decomposed before or during subsequent aluminum filling. Independent claims are also included for the following: (i) a starting mixture of titanium (especially as titanium oxide), carbon (precursor), filler and binder for use in the above process; and (ii) a sacrificial body, consisting of the above starting mixture in pressure stable pressed form, for production of an Al2O3/titanium aluminide composite body.
申请公布号 DE19752775(C1) 申请公布日期 1999.04.29
申请号 DE1997152775 申请日期 1997.11.28
申请人 DAIMLERCHRYSLER AG, 70567 STUTTGART, DE 发明人 RAUSCHER, STEFFEN, DIPL.-ING., 89073 ULM, DE;SCHEYDECKER, MICHAEL, DIPL.-ING., 89278 NERSINGEN, DE;HESSELMANN, CHRISTOPH, 48432 RHEINE, DE;HAUG, TIELMANN, DIPL.-ING., 88690 UHLDINGEN-MUEHLHOFEN, DE
分类号 F16C33/24;B22D17/00;B22D19/00;B22D19/14;B22F1/00;C04B35/46;C04B35/634;C04B35/636;C04B41/51;C04B41/88;C22C1/10;C22C32/00;F16D69/02 主分类号 F16C33/24
代理机构 代理人
主权项
地址