发明名称 POLYARYLENE SULPHIDE FOAMS AND PROCESS FOR PRODUCING THE SAME
摘要 PCT No. PCT/EP95/03080 Sec. 371 Date May 2, 1997 Sec. 102(e) Date May 2, 1997 PCT Filed Aug. 2, 1995 PCT Pub. No. WO96/05246 PCT Pub. Date Feb. 22, 1996A foamed polyarylene sulfide according to the invention has a density which is reduced by at least 50% compared with the theoretical density of nonfoamed material, and is expediently produced by subjecting a polyarylene sulfoxide as such or a mixture of one or more polyarylene sulfides with a polyarylene sulfoxide to heat treatment. The temperature of the heat treatment is in the range from 250 DEG to 400 DEG C.
申请公布号 EP0776344(B1) 申请公布日期 1999.04.07
申请号 EP19950929060 申请日期 1995.08.02
申请人 TICONA GMBH 发明人 FRANK, GEORG;KULPE, JUERGEN;SCHLEICHER, ANDREAS;SCHECKENBACH, HELMUT
分类号 C08G75/18;C08J9/02;C08L81/00;C08L81/02 主分类号 C08G75/18
代理机构 代理人
主权项
地址