发明名称 FASTER TWO-STEP SEALING OF ANODIZED ALUMINUM SURFACES
摘要 Anodized aluminum surfaces are advantageously sealed by an energy- and timesaving two step process, in which the first step is contact at not more than 75 ~C with a solution containing lithium and fluoride ions and, optionaly, surfactant. The second necessary step is treatment with hot water or steam, which may be completed in considerably less time than when only hot water or steam is used for sealing. Conventional smut inhibitors and/or neutral buffers as used in hot water for single step sealing may advantageously be included in the second step of this process. 100 - 1000 ppm concentrations of nickel and/or cobalt ions in the treatment liquid for the second treatment step, if environmentally tolerable, make it possible to complete this step in as little as 10 minutes at a temperature as low as 88 ~C.
申请公布号 CA2300859(A1) 申请公布日期 1999.03.04
申请号 CA19982300859 申请日期 1998.08.19
申请人 HENKEL CORPORATION 发明人 JOHNSON, PHILIP M.;WOJCIECHOWSKI, SCOTT A.;CARLSON, LAWRENCE R.
分类号 C25D11/18;C25D11/24;(IPC1-7):C25D11/18 主分类号 C25D11/18
代理机构 代理人
主权项
地址