发明名称 |
PREPARATION OF SOLID ACID CATALYST |
摘要 |
PROBLEM TO BE SOLVED: To provide a method of preparing a molded solid acid catalyst having a high activity equivalent to or higher than that of a powder catalyst even though it is made as a solid acid catalyst molding containing a sulfuric acid constituent. SOLUTION: (a) Zirconium hydroxide and/or hydrate and aluminum hydrate having a boemite structure are mixed with each other and a molding is formed. (b) Then, the molding is burned at a temperature at which tetragonal zirconia is obtained. (c) The molding is made to carry a sulfuric acid constituent containing compound and is burned at a temperature of 300 deg.C or higher and lower than 700 deg.C. |
申请公布号 |
JPH1157478(A) |
申请公布日期 |
1999.03.02 |
申请号 |
JP19970243528 |
申请日期 |
1997.08.26 |
申请人 |
JAPAN ENERGY CORP |
发明人 |
MATSUZAWA KENJI;SEKI KAZUHIRO |
分类号 |
B01J27/053;C07B61/00;C07C5/22;C07C13/18 |
主分类号 |
B01J27/053 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|