<p>Preparation of active silicon powder for use in the Rochow reaction is claimed, in which metallurgical Si, containing more than 98% of Si, up to 0.4% Fe, up to 0.2% Al and up to 0.2% Ca, is milled to a particle size of less than 350 microns in the presence of at least one catalyst and/or promoter of the reaction.The operation is carried out so as to distribute the element(s) on the surface of the particles. Also claimed, is the activated Si powder , having a surface coating of catalytic elements.</p> |