发明名称 |
MIXTURE FOR INDUCTION WELDING DEPOSITION OF WEAR-RESISTANT MATERIAL |
摘要 |
FIELD: welding. SUBSTANCE: mixture contains, wt %: austenite chromium-manganese steel (carbon content 0.1-0.35), 55.0-70.0; austenite manganese cast iron, 18.0-33.0; and flux based on boron- containing components, 12.0-15.0. EFFECT: increased dynamic strength under abrasive friction conditions with impact loads and improved soldering conditions due to lowered melting temperature of mixture excluding overheating of basic metal. 2 tblq
|
申请公布号 |
RU2123920(C1) |
申请公布日期 |
1998.12.27 |
申请号 |
RU19970116596 |
申请日期 |
1997.10.01 |
申请人 |
ALTAJSKIJ GOSUDARSTVENNYJ TEKHNICHESKIJ UNIVERSITE;T IM I I POLZUNOVA |
发明人 |
EVSTIGNEEV V.V.;SACHAVSKAJA N.A.;STAROSTENKOV M.D.;SACHAVSKIJ A.A. |
分类号 |
B23K35/36;(IPC1-7):B23K35/36 |
主分类号 |
B23K35/36 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|