发明名称 Thermally stable polyoxymethylene copolymer
摘要 A polyoxymethylene copolymer prepared by copolymerizing a mixture comprising trioxane and 1,3-dioxolane in the presence of at least one polymerization catalyst selected from the group consisting of boron trifluoride, a boron trifluoride hydrate and a coordination complex compound of an organic compound containing an oxygen atom or a sulfur atom with boron trifluoride, wherein the 1,3-dioxolane has a 2-methyl-1,3-dioxolane content of not more than 500 ppm by weight and a 1,3-dioxolane peroxide content of not more than 15 ppm by weight in terms of hydrogen peroxide, and contains at least one hindered phenol in an amount of from 10 to 500 ppm by weight, each based on the weight of the 1,3-dioxolane.
申请公布号 US5837781(A) 申请公布日期 1998.11.17
申请号 US19970804507 申请日期 1997.02.24
申请人 ASAHI KASEI KOGYO KABUSHIKI KAISHA 发明人 TANIMURA, NORITAKA;TANIGAWA, YUKIO
分类号 C08G2/10;C08G2/18;C08G2/24;(IPC1-7):C08L61/02;C08G4/00;C08G6/00 主分类号 C08G2/10