发明名称 |
METHOD FOR THERMAL TREATMENT OF GRANULATED IRON ORE BEFORE REDUCTION |
摘要 |
<p>The wet granulated iron ore is initially conducted through a drying zone. The ore leaves the drying zone at a temperature of 120-400 ~C. The ore is then heated in direct contact with hot gas to temperatures of 700-1,100 ~C before being delivered to a reduction zone. The ore coming out of the drying zone is fully or partially guided through a separating device so as to separate the ore into fine and coarse grain fractions. The fine-grained ore fraction is conveyed to a granulating device so as to produce an iron ore granulate which is conducted to the drying zone. The coarse-grained ore fraction is heated to temperatures of 700-1,100 ~C before it is guided into the reduction zone.</p> |
申请公布号 |
CA2288217(A1) |
申请公布日期 |
1998.11.05 |
申请号 |
CA19982288217 |
申请日期 |
1998.04.17 |
申请人 |
METALLGESELLSCHAFT AKTIENGESELLSCHAFT |
发明人 |
BEYZAVI, ALI;HIRSCH, MARTIN |
分类号 |
B01J8/18;C21B13/00;C22B5/14;(IPC1-7):C21B13/00 |
主分类号 |
B01J8/18 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|