摘要 |
The invention relates to tissue products having improved softness properties and methods of making them. Specifically, improved softness is achieved by incorporating one or more softeners/debonders into the fiber furnish at the wet end of the tissue machine prior to formation, followed by a topical treatment with one or more softeners/debonders after the tissue web is dried. The result is a tissue product with added bulk and a smooth surface feel, both properties contributing to improved softness characteristics.
|