PROBLEM TO BE SOLVED: To obtain an olefin resin foam excellent in flame retardancy and moldability and having good appearance. SOLUTION: This foam comprises 100 pts.wt. olefin resin comprising 30-90wt.% propylene resin showing an eluate amount of 75-90wt.% at 94 deg.C or above as measured by cross fractionation and an eluate amount of 60-75wt.% at 100 deg.C or above and a melt index of 0.2-5g/10min and 10-70wt.% ethylene resin, 1-100 pts.wt. bromine-containing compound and 0.1-10 pts.wt. antimony trioxide. |