摘要 |
<p>Disclosed is a method for increasing the charring ratio of coal. In manufacturing an ingot iron using the coal, magnesium oxide or limestone is used as an additive for charring the coal. The additive increases the charring ratio of the coal while giving no affection onto slag. An MgO suspension or limestone suspension is mixed with the coal and thus obtained mixture is dried to attach MgO or the limestone onto the surface of the coal. The charring effect is increased and the using amount of coke can be reduced.</p> |