发明名称 High internal pressure forming of aluminum alloy hollow bodies
摘要 An alloy suitable for manufacturing components out of a hollow body by high internal pressure forming contains, in wt. %, - Silicon 0.3 to 1.6 - Magnesium 0.3 to 1.3 - Iron max. 0.5 - Copper max. 0.9 - Manganese max. 0.5 - Vanadium 0.05 to 0.3 - Cobalt max. 0.3 - Chromium max. 0.3 - Nickel max.0.8 - Zirconium max. 0.3 - and other alloying elements, individually at most 0.05, in total at most 0.15, the remainder aluminum.
申请公布号 US5766546(A) 申请公布日期 1998.06.16
申请号 US19970816542 申请日期 1997.03.13
申请人 ALUSUISSE TECHNOLOGY & MANAGEMENT LTD. 发明人 SCHWELLINGER, PIUS
分类号 C22F1/00;B21D26/02;B21D26/053;C22C21/02;C22C21/06;C22C21/08;C22F1/05;(IPC1-7):C22C21/08 主分类号 C22F1/00