发明名称 |
METHOD OF LOW-DEFORMATION HARDENING AFTER NITROCEMENTATION |
摘要 |
FIELD: mechanical engineering. SUBSTANCE: invention relates to manufacturing parts with nitrocementation (cementation) with low allowances for mechanical conversion after heat treatment. Cooling time from austenitization temperature to 100 C is determined for one part belonging to serial manufacture party. The part is hardened in cold oil to 100 C, transferred into boiling water, held there for 10- 15 min, and then cooled in air. EFFECT: extended production possibilities of low-deformation hardening in oil and reduced strains. 2 tbl(
|
申请公布号 |
RU2112811(C1) |
申请公布日期 |
1998.06.10 |
申请号 |
RU19960119897 |
申请日期 |
1996.10.03 |
申请人 |
KOMBINAT "EHLEKTROKHIMPRIBOR" |
发明人 |
KARPOV L.P.;SUKHANTSEV A.G. |
分类号 |
C21D1/58;C23F17/00;(IPC1-7):C21D1/58 |
主分类号 |
C21D1/58 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|