发明名称 COPPER ALLOY AND PROCESS FOR OBTAINING SAME
摘要 A copper base alloy consisting essentially of tin in an amount from about 1.0 to 11.0 % by weight, phosphorous in an amount from about 0.01 to 0.35 % by weight, iron in an amount from about 0.01 to about 0.8 % by weight, optionally up to 15 wt.% zinc, and the balance essentially copper, including phosphide particles uniformly distributed throughout the matrix, is described. The alloy is characterized by an excellent combination of physical properties. The process of forming the copper base alloy described herein includes casting, homogenizing, rolling, process annealing and stress relief annealing.
申请公布号 WO9820176(A1) 申请公布日期 1998.05.14
申请号 WO1997US13747 申请日期 1997.08.05
申请人 WATERBURY ROLLING MILLS, INC. 发明人 BHARGAVA, ASHOK, K.
分类号 C22C9/02;C22C9/04;C22F1/00;C22F1/08;H01B1/02 主分类号 C22C9/02
代理机构 代理人
主权项
地址