发明名称 Method of making calcification-resistant bioprosthetic tissue
摘要 A method of treating a collagenous biomaterial, such as porcine aortic valve leaflets or bovine pericardium, by exposing the biomaterial to an alcohol to inhibit in vivo calcification. The biomaterial, preferably glutaraldehyde-pretreated, is subjected to an aqueous solution of 60% to 80% lower aliphatic alcohol, such as ethanol for a period of at least 20 minutes, and preferably, 24 to 72 hours. The biomaterial is rinsed, and then stored in either a glutaraldehyde-free environment or an ethanolic solution of glutaraldehyde. In some embodiments, the treatment solutions include an additional anticalcification agent which may be a soluble salt of a metallic cation, such as Al+3 or Fe+3.
申请公布号 US5746775(A) 申请公布日期 1998.05.05
申请号 US19930140722 申请日期 1993.10.21
申请人 THE BOARD OF REGENT6S OF THE UNIVERSITY OF MICHIGAN 发明人 LEVY, ROBERT J.;HIRSCH, DANIELLE
分类号 A61L2/16;A61L27/00;A61L27/36;A61L27/50;A61L27/54;C14C3/00;C14C3/04;(IPC1-7):A61F2/02;A61F2/24;D01C3/00 主分类号 A61L2/16
代理机构 代理人
主权项
地址