<p>The present invention provides an anisotropically porous membrane which is obtained according to a wet process, which comprises a substantially non-sulfonated aromatic polyether ketone having a crystallinity of 10 percent by weight or higher, and which has open pores having an average pore diameter of 0.02 to 30.00 mu m on both surfaces of said membrane at an open pore ratio of 7 to 90 percent. In accordance with the present invention, a porous crystalline aromatic polyether ketone membrane is provided which is excellent in heat resistance, chemical resistance, water resistance, water permeability and a balance of water permeability and fractionating characteristics. <IMAGE></p> |