发明名称 Corrective tempering method and apparatus for rolling elements.
摘要 In a corrective tempering method and apparatus for a rolling element in which the thermal deformation of the rolling element is corrected within an extremely short time by utilizing plasticity exhibited during a metallic structure transforming process brought about by low-temperature tempering of the rolling element made of steel, the hardened rolling element is heated and pressured to a maximum temperature within a range of from 250 to 500° C. by a heating device while set in correcting molds to correct the deformation of the rolling element at a degree of working within a range not exceeding an elastic deformation range of the rolling element at a room temperature. The rolling element can be heated also by an induction heating device in addition to a conduction heating device. A product whose inner/outer diameter correcting degree of deformation is 60% or more, dimension standardizing rate is 30% or more, surface roughness is less than Ra 0.2 mum, and surface hardness is HRC 56 or more can be obtained for a correction time within 6 minutes and an induction heating time within 30 seconds.
申请公布号 GB2297766(B) 申请公布日期 1998.02.25
申请号 GB19960008464 申请日期 1995.08.23
申请人 * NSK LTD 发明人 KIYOSHI * HIRAKAWA;AKITOSHI * MAEDA;HIROAKI * SUGIYAMA;MANABU * OHHORI
分类号 C21D1/26;C21D1/30;C21D1/40;C21D1/42;C21D1/673;C21D9/40 主分类号 C21D1/26
代理机构 代理人
主权项
地址