摘要 |
A batch process for increasing the calcium content of a water solution comprises the placement of a tin catalyst, a glass fibrous material, and water into a sealed tank and the application of heat to the tank for predetermined time intervals at progressively decreasing temperatures. The resulting solution is then extracted from the tank, wherein the solution has between 200 ppm and 500 ppm concentration of calcium.
|