摘要 |
<p>PROBLEM TO BE SOLVED: To provide sufficient slip properties and antistatic properties even when an adding amount of an additive is small and flame treatment is not carried out. SOLUTION: In the multilayer glossy plastic container structured so that at least two resin layers are laminated, the most outer layer of the resin layer is composed of a resin composition containing high pressure method low density polyethylene of 95-110 deg.C melting point (A), aliphatic amide (B), and at least one kind of a compound (C) selected from a group consisting of N,N-bis(2- hydroxyethyl)alkylamine, N,N-bis(2-hydroxyethyl)aliphatic amide, and glycerol aliphatic ester. An added amount (b) (pts.wt.) of the aliphatic amide (B) and an added amount (C) (pts.wt.) of the compound (C) satisfy the formula b+0.025<=c<=b+0.175, 0.01<=b<=0.1 to 100 pts.wt. of the polyethylene (A).</p> |