发明名称 |
METHOD FOR COOLING CONTINUOUSLY CAST BLOOM |
摘要 |
PROBLEM TO BE SOLVED: To provide a cooling method capable of preventing the occurrence of surface flaw over the whole surface caused at the time of cooling a continuously cast bloom. SOLUTION: When the bloom cast by a continuous casting is cut into prescribed length, then cooled from the temp. range just above Ar3 transformation point while being placed in the horizontal direction by using a bloom cooler installed at the outside of the continuous casting machine, the bloom is cooled by controlling the water quantity density on the upper surface of the bloom to 5×10<-4> to 4×10<-3> m<3> /sm<2> , that on the side surface thereof to >=1.5 times of that on the upper surface, and that on the lower surface thereof to >=2.0 times of that on the upper surface.
|
申请公布号 |
JPH101719(A) |
申请公布日期 |
1998.01.06 |
申请号 |
JP19960171754 |
申请日期 |
1996.06.10 |
申请人 |
SANYO SPECIAL STEEL CO LTD |
发明人 |
NURI YOSHIO;KATO YOSHIYUKI |
分类号 |
B22D11/124;B22D11/22;C21D1/00;C21D1/84;C21D9/00;(IPC1-7):C21D1/00 |
主分类号 |
B22D11/124 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|