摘要 |
The glaze mixing preventive pigment is prepared by mixing 60-70 wt.% of petroleum distillate, 20-25 wt.% of bronze powder, 8-12 wt.% of starch powder and 2-5 wt.% of pigment; heating the solid mixture at 100-120 degrees centigrade for about 10 minutes; adding 55-65 wt.% of cellulose ester, 15-20 wt.% of diacetone alcohol and 3-8 wt.% of silica to 15-20 wt.% of the mixture solution; and naturally drying the mixture.
|