发明名称 |
PRODUCTION OF THERMOPLASTIC RESIN FILM EXCELLENT IN INK DRYING |
摘要 |
PROBLEM TO BE SOLVED: To obtain a synthetic paper requiring a short drying time and excellent in adherence of ink by using a widely used oily ink. SOLUTION: A resin which is a mixture of a component B): 8-350 pts.wt. of an inorganic fine powder having an average particle diameter 0.01-10μm and a component A): 100 pts.wt. of a thermoplastic resin is a base wood of a stretched film. And the stretched film is kept in a stretched state. A support with a sharp angle of a tip part is abutted to a surface of this stretched material approximately in parallel to a direction of stretch and the stretched material is bended partially and the bending angle is determined to a deformation area with 50-140 degree. A continuous striping craze is formed approximately at right angle to a moving direction by relatively moving the film in order and the surface of the stretched material with the craze is oxidized. |
申请公布号 |
JPH09300477(A) |
申请公布日期 |
1997.11.25 |
申请号 |
JP19960146475 |
申请日期 |
1996.05.17 |
申请人 |
OJI YUKA SYNTHETIC PAPER CO LTD;MITSUBISHI CHEM CORP |
发明人 |
SHIBUYA SANEHIRO;OCHIAI HISAO;KITAMURA KAZUHISA;SANO HIROSHIGE;UCHIYAMA YUKIO;IKEHATA FUMIYO |
分类号 |
C08J7/00;B29C55/02;B29D7/00;B29K23/00;B29L7/00;(IPC1-7):B29D7/00 |
主分类号 |
C08J7/00 |
代理机构 |
|
代理人 |
|
主权项 |
|
地址 |
|